N08367

Facebook
Twitter
LinkedIn

Description

Our company’s scope of supply includes

Non-standard forgings, round rods, steel plates/steel belts, flange pipe fittings, seamless pipes, capillaries, etc. Welcome to inquire!

1. Introduction to N08367 Materials

      N08367 is a typical 6-molybdenum (high molybdenum content 6.3%) super austenitic stainless steel. Its ability to resist chloride pitting, crevice corrosion and stress corrosion is better than that of series 3 stainless steel and has a lower cost than corrosion-resistant nickel-based alloys. It exhibits good corrosion resistance in various severe corrosion environments and is suitable for high chloride aqueous solutions and chloride corrosion environments. Its comprehensive corrosion resistance has made a great leap compared to 316L. At the same time, its corrosion resistance is close to that of other corrosion-resistant nickel-based alloys such as C-276, but its cost is more advantageous. Used in a variety of high chloride environments: bleaching agents (nano hypochlorite, chlorine dioxide), halogen and chemicals with high salt or seawater content.

2. N08367 chemical composition

alloy % C And Mn P S In Cr Mo Cu N
N08367 Minimum value 23.5 20.0 6.0 0.18
Maximum value 0.03 1.0 2.0 0.040 0.030 25.5 22.0 7.0 0.75 0.25

 3. N08367 physical properties

Specific heat (J/kg-K) 450
Resistivity (μΩ-cm) 94.4
Thermal conductivity (W/mK) 20℃ 11.9
100℃ 13.0
Average thermal expansion coefficient (10-6/℃) 20–200℃ 15.3
20–300℃ 15.6
20–400℃ 15.9
20–500℃ 16.2
Longitudinal elastic modulus (MPa) 19.8 x 104
density 8.24
Melting point (℃) 1360-1394

       N08367 Heat treatment

      This alloy is an austenitic series stainless steel, and the heat treatment can be the same as that of standard austenitic stainless steel. The commonly used heat treatment conditions are as follows.

      Solid solution treatment 1125~1175℃ water cooling

      N08367 Pickling

      Use a mixture of nitric acid and hydrofluoric acid for pickling. Due to its higher corrosion resistance than SUS 304, the scale will be slightly more difficult to remove. Therefore, it is more effective to perform a short period of alkali impregnation before pickling, or if possible shot peening.

IV. N08367 application fields

  1. Seawater environment: seawater desalination device, seawater heat exchanger, condenser tube, etc.
  2. High-concentration chloride ion environment: smoke exhaust desulfurization device, pulp and paper industry, various bleaching devices, etc.
  3. Environment containing high concentration of salt: resin manufacturing equipment, chemical reaction containers and pipes, etc.
  4. Flue gas desulfurization equipment (FGD), crude oil distillation tower and filler for storage tanks and pressure rollers, thermal power plants, steel plants, and petrochemical enterprises,
  5. Pharmaceutical equipment, food machinery equipment
Scroll to Top