GH5188

카테고리
Facebook
트위터
LinkedIn

설명

항공 그룹에 대한 공급 범위

단조품, 원형 막대, 강판, 링, 이음매없는 파이프, 강판 / 스틸 벨트, 와이어 용접 재료, 문의 환영합니다!

1. 소개 GH5188 자료

       GH5188 is a Co-Ni-Cr-based solid solution reinforced deformation high-temperature alloy with a use temperature of less than 1100℃. Add 14% w(W) to the alloy for solid solution strengthening, so that the alloy has good comprehensive performance; add a higher content of chromium and trace lanthanum to make the alloy have good high-temperature oxidation resistance. The alloy has good process properties such as hot and cold processing plasticity and welding, and is suitable for making aircraft engine parts that require high strength below 980℃ and require oxidation resistance below 1100℃.

       GH5188 can produce and supply various deformation products, such as thin plates, medium plates, strips, bars, forgings, silk materials and precision castings.

2. 화학 성분

합금 % C Cr In Co W Fe B The 그리고 P S Cu Ag Bi Pb Mn
GH5188 최소값 0.05 20.0 20.0 margin 13.0 0.03 0.2
최대 값 0.15 24.0 24.0 16.0 3.0 0.015 0.012 0.5 0.020 0.015 0.07 0.001 0.0001 0.001 1.25

3. Technical standards of GH5188 (GH188) materials    

      GH5188GJB 3317-1998 “Specifications for Hot Rolled Plates for High Temperature Alloys for Aviation”

      GH5188Z9 0103-1990 “Technical Conditions of GH188 Alloy Plate”

      GH5188Z9 132-1999 “Technical Conditions for Cold Drawing of GH188 Alloy for Welding”

      GH5188Q/5B 4002-1992 “GH188 Alloy Cold Rolled Strip”

      GH5188Q/5B 4003-1992 “GH188 Alloy Cold Rolled Plate”

      GH5188Q/5B 4014-1992 “Technical Conditions of GH188 Alloy Forging”

      GH5188Q/5B 4020-1992 “K188 Alloy Investment Precision Casting”

      GH5188Q/5B 4022-1992 “GH188 Alloy Rod”

      GH5188Q/5B 4057-1992 “GH188 High Temperature Alloy Cold-Tear Welding Wire”

 IV. Physical properties

밀도  녹는점 
g / cm3
9.09 1300-1360

V. Application areas

      High-temperature components such as flame cylinders and guide blades in the combustion chamber of aircraft engines are well produced and used.

      Aero engine parts that require high strength below 980℃ and require antioxidant below 1100℃.

      The corrosion resistance of alloy sheets is better than that of GH3536 alloy.