Beschreibung
Lieferumfang der Aviation Group:
Nicht standardisierte Schmiedestücke, Rundstangen, Stahlplatten, Ringe, nahtlose Rohre
- 17-4PH material introduction
17-4PH alloy is precipitated, hardened, martensite stainless steel composed of copper, niobium/cinnabar.
Corresponding grade: 0Cr17Ni4Cu4Nb 05Cr17Ni4Cu4Nb S17400
- 17-4PH chemical composition
| Legierung | % | C | Mn | Und | P | S | Cr | Unter | Cu | Fe | Nb |
| 17-4ph | Minimaler Wert | – | – | – | – | – | 15.5 | 3.0 | 3.0 | Marge | 0.15 |
| Maximaler Wert | 0.07 | 1.0 | 1.0 | 0.040 | 0.030 | 17.5 | 5.0 | 5.0 | 0.45 |
- 17-4PH physical properties
| Dichte | 7,78 g/cm3 |
| Schmelzpunkt | 1400-1440℃ |
Mechanical properties of 17-4PH alloy at room temperature:
| Legierung | Zugfestigkeit Rm N/mm2 |
Streckgrenze RP0.2N/mm2 |
Dehnung A5 % |
Brinell-Härte HB |
| 480℃ Alterung | ≥1310 | ≥1180 | ≥10 | ≥40 |
| 550℃ Alterung | ≥1060 | ≥1000 | ≥12 | ≥35 |
| 580℃ Alterung | ≥1000 | ≥865 | ≥13 | ≥31 |
| Alterungseffekt von 620℃ | ≥930 | ≥325 | ≥16 | ≥28 |
- 17-4PH corrosion resistance
- The corrosion resistance of 17-4PH alloy is better than any other standard hardenable stainless steel plate. In most cases, its corrosion resistance is no less than 304.
- Besteht die Gefahr von Spannungsrisskorrosion, muss die höhere Alterungstemperatur über 550°C (1022°F), vorzugsweise 590°C (1094°F), liegen.
- Die Anlasstemperatur im Chloridmedium beträgt 550°C-1022°F.
- Die Anlasstemperatur im H2S-Medium beträgt 590°C-1094°F.
- Es ist anfällig für Korrosion oder Risskorrosion in statischem Seewasser.
- Seine Korrosionsbeständigkeit ist die gleiche wie die der Sorte 304L in der Petrochemie, Lebensmittel- und Papierindustrie.
- 17-4PH application fields
- Maritime Plattform, Hubschrauberdeck, andere Plattformen
- Lebensmittelindustrie
- Zellstoff- und Papierindustrie
- Luft- und Raumfahrt (Turbinenschaufeln)
- Mechanische Komponenten